Evaluating anisotropic properties in the porcine temporomandibular joint disc using nanoindentation.
Yuya PA; Amborn EK; Beatty MW; Turner JA; Annals Of Biomedical Engineering, 2010, vol. 38, issue 7, p 2428, ISSN 15739686. ISBN 15739686.